TL;DRAbstract

The results of galvanic testing were varied in each environment. The position of metals in the galvanic series was not fixed, but changed with environment. In all cases where high general and galvanic corrosion rates were observed, the conditions of potential, pH, and impurity content could be correlated with regions of oxide surface film instability outlined by Pourbaix Diagrams. The majority of the severe corrosion reactions were observed in the acidic environment, although a few were noted in the caustic environment. The presence of chlorides tended to enhance galvanic corrosion rates at the neutral environment. 10 tables.

Chat with Paper

AI Agents for this Paper

The results of galvanic testing were varied in each environment. The position of metals in the galvanic series was not fixed, but changed with environment. In all cases where high general and galvanic corrosion rates were observed, the conditions of potential, pH, and impurity content could be correlated with regions of oxide surface film instability outlined by Pourbaix Diagrams. The majority of the severe corrosion reactions were observed in the acidic environment, although a few were noted in the caustic environment. The presence of chlorides tended to enhance galvanic corrosion rates at the neutral environment. 10 tables.

Keywords

Galvanic cellUraniumCorrosionGalvanic corrosionMetallurgyEnvironmental scienceMaterials scienceEnvironmental chemistry

Chat

Click to start Chat