Studi Metalografi Pengaruh Arus Dan Holding Time Pada Pengelasan Spot Welding Material Stainless Steel

Rinomo Muhammad Fahmi,Muhammad Alfatih Hendrawan,MT Ir. Masyrukan-2015-01-01-UMS Library Center of Academic Activities (Universitas Surakarta)

TL;DRAbstract

In the spot welding process, namely process of joining two or more metal plates, there are many factors that must be considered. Welding current, electrical resistance, and the welding time is a major factor in the welding point. These factors may affect the quality of the weld. However, it is possible there are other factors that also affect the quality of the welding, one of which is the welding cycle including the holding time.
\nThis study aims to identify the chemical composition of the metal plate used in welding spot welding and also to observe the influence of currents and holding time physically with macro and micro observations photo area parent metal, HAZ, and weld metal regions. The material used in this study is stainless steel with a thickness of 0.8 mm. The parameters used in this study is the welding current 5 kA, 6 kA, and 7 kA, constant welding time of 0.3 seconds, with a variation of holding time of 1 second, 3 seconds, and 5 seconds.
\nTest showed that the c

Chat with Paper

AI Agents for this Paper

In the spot welding process, namely process of joining two or more metal plates, there are many factors that must be considered. Welding current, electrical resistance, and the welding time is a major factor in the welding point. These factors may affect the quality of the weld. However, it is possible there are other factors that also affect the quality of the welding, one of which is the welding cycle including the holding time.
\nThis study aims to identify the chemical composition of the metal plate used in welding spot welding and also to observe the influence of currents and holding time physically with macro and micro observations photo area parent metal, HAZ, and weld metal regions. The material used in this study is stainless steel with a thickness of 0.8 mm. The parameters used in this study is the welding current 5 kA, 6 kA, and 7 kA, constant welding time of 0.3 seconds, with a variation of holding time of 1 second, 3 seconds, and 5 seconds.
\nTest showed that the c

Keywords

WeldingMaterials scienceMetallurgyHeat-affected zoneSpot weldingElectric resistance weldingFlash weldingShielded metal arc welding