Joining magnetic alloy 49Fe--49Co--2V to 304L stainless steel. Technical Spinoff Report

D.M. Jarboe-1973-08-01
0

TL;DRAbstract

conventionally processed bar. Soft magnetic properties were assessed through B-H hysteresis curves from which coercivity (Hc) values were extracted. Hc decreases rapidly with annealing above 650°C as well, i.e. improved soft magnetic behavior. The observed trend is attributed to annealing and grain growth in this temperature regime, which facilitates magnetic domain wall movement. The coercivity vs. grain size results generally follow the trend predicted in the literature. The magnetic behavior of annealed ECAE material compares favorably to conventional bar, possibly due to mild crystallographic texturing which enhances properties in the post-ECAE annealed material. Overall, this study highlights a definitive tradeoff between mechanical and magnetic properties brought about by post-ECAE annealing and grain growth.

Chat with Paper

AI Agents for this Paper

conventionally processed bar. Soft magnetic properties were assessed through B-H hysteresis curves from which coercivity (Hc) values were extracted. Hc decreases rapidly with annealing above 650°C as well, i.e. improved soft magnetic behavior. The observed trend is attributed to annealing and grain growth in this temperature regime, which facilitates magnetic domain wall movement. The coercivity vs. grain size results generally follow the trend predicted in the literature. The magnetic behavior of annealed ECAE material compares favorably to conventional bar, possibly due to mild crystallographic texturing which enhances properties in the post-ECAE annealed material. Overall, this study highlights a definitive tradeoff between mechanical and magnetic properties brought about by post-ECAE annealing and grain growth.

Keywords

CoercivityAnnealing (glass)Materials scienceGrain sizeAlloyMetallurgyGrain growthMagnetic hysteresis

Chat

Click to start Chat