THE PREPARATION OF LARGE-DIAMETER ZIRCONIUM CRYSTAL BAR BY THE DE BOER PROCESS
TL;DRAbstract
From introduction: "This is the ninth monthly report, BMI-514, under Contract No. AT(30-1)-771 on "Zirconium Research and Development". The report covers the work period from September 15, 1950, to October 15, 1950. Work is continuing on the preparation of large-diameter zirconium crystal bars in the 16-inch-diameter de Boer unit. Crystal bars up to 1-5/16 inches in diameter and 8 feet long have been prepared in this unit."
Chat with Paper
AI Agents for this Paper
From introduction: "This is the ninth monthly report, BMI-514, under Contract No. AT(30-1)-771 on "Zirconium Research and Development". The report covers the work period from September 15, 1950, to October 15, 1950. Work is continuing on the preparation of large-diameter zirconium crystal bars in the 16-inch-diameter de Boer unit. Crystal bars up to 1-5/16 inches in diameter and 8 feet long have been prepared in this unit."