TL;DRAbstract

The purpose of this study was to evaluate the tensile bond strength of conventional dentin adhesive systems and self-etching primers at 10 minute and 24 hours.Flat dentin surfaces were prepared on labial surface of 120 bovine lower incisor teeth and a 4-mm-diameter bonding area was demarcated on each prepared surface with adhesive vinyl tape.In the following groups were applied the dentin systems and the composite resin Z 1 00: Groups A and B -ScotchBond Multi-Purpose Plus and Z 100; Groups C and D-Single Bond; Groups E and F-Ciearfil Liner Bond 2V and Groups G and H-Clearfil SE Bond.In the groups A, B, C and D ali dentin was etched with 35% phosphoric acid, washed and the excess of water was removed.A resin composite rod was positioned on the bonding area and cured for 20 s at the three points of the interface to perform the tensile bond strength (TBS).The TBS was tested at 10 minute to groups A, C, E and G.The groups B, D, F and H were stored in distilled water at 3rC and the TBS was

Chat with Paper

AI Agents for this Paper

The purpose of this study was to evaluate the tensile bond strength of conventional dentin adhesive systems and self-etching primers at 10 minute and 24 hours.Flat dentin surfaces were prepared on labial surface of 120 bovine lower incisor teeth and a 4-mm-diameter bonding area was demarcated on each prepared surface with adhesive vinyl tape.In the following groups were applied the dentin systems and the composite resin Z 1 00: Groups A and B -ScotchBond Multi-Purpose Plus and Z 100; Groups C and D-Single Bond; Groups E and F-Ciearfil Liner Bond 2V and Groups G and H-Clearfil SE Bond.In the groups A, B, C and D ali dentin was etched with 35% phosphoric acid, washed and the excess of water was removed.A resin composite rod was positioned on the bonding area and cured for 20 s at the three points of the interface to perform the tensile bond strength (TBS).The TBS was tested at 10 minute to groups A, C, E and G.The groups B, D, F and H were stored in distilled water at 3rC and the TBS was

Keywords

DentinUltimate tensile strengthBond strengthAdhesiveMaterials sciencePhosphoric acidComposite numberUniversal testing machine

Chat

Click to start Chat