Assessment of stress corrosion cracking and hydrogen embrittlement susceptibility of buried pipeline steels
Alysson Helton Santos Bueno,B. B. Castro,José Antônio da Cunha Ponciano Gomes-2008-01-01-Elsevier eBooks